Natural Fibre Hybrid Composite for a Scooty Front Panel: Effect of Fibre Length and Alkali Treatment on Flexural and Tensile Strength

A composite combines a stiff reinforcing phase – fibres, sheets or particles – with a tougher matrix that holds it together and transfers the load. Natural fibres such as kenaf and similar plant fibres are cheap, renewable, light and biodegradable, which makes them attractive for non-structural vehicle parts such as panels and covers.

This project develops short natural-fibre hybrid composites with an epoxy matrix for use in a scooty front panel, and studies how fibre length and alkali (NaOH) treatment change their strength.

Making the Laminates

  • Fibres chopped to 4 mm, 8 mm and 12 mm lengths
  • Half of the fibres alkali-treated in a dilute sodium hydroxide solution to clean and roughen their surface
  • Hand lay-up in a mould coated with wax and PVA release agent
  • A load of 1000 N applied on the top plate for about 24 hours while the epoxy cures

Natural fibres keep their strength up to about 160 °C, so curing was kept below this temperature.

Flexural Test Results

Specimens of 62 mm × 12 mm × 5 mm were tested at a crosshead speed of 3 mm/min, five specimens per laminate.

FibresMax. deflection (mm)Max. load (N)Max. flexural strength (MPa)
4 mm treated1.6126.239.12
4 mm untreated1.4108.233.54
8 mm treated1.8154.447.86
8 mm untreated1.6124.838.69
12 mm treated1.6134.241.60
12 mm untreated2.0118.036.85

Tensile Test Results

Fibre lengthPeak load (N)Ultimate tensile strength (MPa)
4 mm treated38010.86
4 mm untreated61016.60
8 mm treated53013.57
8 mm untreated62020.24
12 mm treated64014.68
12 mm untreated47014.30

The 8 mm alkali-treated fibres gave the highest flexural strength, 47.86 MPa at a load of 154.4 N. Alkali treatment raised the flexural strength for every fibre length. In tension the trend is different, which is common in short-fibre composites where fibre orientation and bonding control the result – how to read these results is discussed in the live class.

Why Natural Fibre Composites

Vehicle makers are under pressure to cut weight and use renewable materials. Natural fibre composites can replace glass-fibre or plastic parts in door panels, dashboards and covers, reducing weight and environmental impact. Their weaknesses – moisture absorption and variable fibre quality – are what treatments such as alkali washing aim to improve.

Real-World Applications

  • Two-wheeler and car interior and body panels
  • Furniture, packaging and building boards
  • Eco-friendly consumer product housings

Related Projects

Explore more design and analysis projects on similar topics:

What Support You Get

  • Design guidance: how to build the CAD model yourself – scooty front panel model and specimen geometry (62 × 12 × 5 mm) for testing
  • Analysis guidance: how to set up and run the analysis yourself – flexural and tensile testing of six laminate types following ASTM standards
  • Report guidance: how to structure your own report – methodology, results and conclusion
  • Live class: a step-by-step explanation of the method while you work on your own licensed software, so you can understand it and present your work confidently

Studying abroad? We guide you too – learn to build projects like this in our live classes, on your own licensed software.

Who Is This Project For?

This natural-fibre hybrid composite project is a good learning example for B.Tech and B.E. final year students, diploma students who want to learn design and analysis, and M.Tech students who want to learn a method they can extend in their own thesis. It is also useful for anyone who wants to learn how natural fibre composites are made and tested as an alternative to plastics on a real engineering problem instead of a textbook example.

Frequently Asked Questions

Which fibre lengths are studied?

4 mm, 8 mm and 12 mm short fibres, each alkali-treated and untreated.

Which composite has the highest flexural strength?

The 8 mm alkali-treated fibre composite, at 47.86 MPa.

What is alkali treatment?

Soaking the fibres in a dilute sodium hydroxide solution to clean and roughen their surface so they bond better with the resin.

Can I learn the natural-fibre hybrid composite project with Engineers R World?

Yes. We teach the method step by step in live classes or recorded videos, and you build the model and run the analysis yourself on your own licensed or free software.

Learn the Natural-fibre Hybrid Composite Project With Us

Want to learn the natural-fibre hybrid composite project for your final year, mini project or M.Tech work? Message us with your university, branch and deadline, and we will share a learning plan – live classes and step-by-step guidance while you build it yourself.

Enquire about this project on WhatsApp or use the enquiry form on our home page. Browse more mechanical projects or 60+ mechanical engineering project ideas.

Interested in this project? Get the details, files and guidance from our team.

Enquire on WhatsApp

Leave a Comment

Your email address will not be published. Required fields are marked *

Scroll to Top